Inconel 625 vs 718: Which Superalloy for Your Application?

Inconel 625 vs 718 infographic comparing corrosion resistance, mechanical properties, high-temperature performance, weldability, applications, and material selection guide by Huaxiao Metal

Choosing the right nickel-based superalloy is critical for ensuring long-term performance, reliability, and cost efficiency in demanding environments. Although Inconel 625 vs 718 are both high-performance nickel alloys developed for extreme temperatures and corrosive conditions, they are engineered with different priorities.

If you need the short answer: choose Inconel 625 when your priority is corrosion resistance — seawater, acids, chlorides, oxidizing environments. The 9% molybdenum in 625 gives it a PREN (Pitting Resistance Equivalent Number) of ≥ 48, making it virtually immune to pitting and crevice corrosion in marine service. Choose Inconel 718 when your priority is high-temperature strength — jet engines, gas turbines, cryogenic valves, or any application above 540°C where you need the strongest nickel alloy commercially available (1375 MPa tensile strength).

This article provides a detailed comparison of Inconel 625 vs Inconel 718, two nickel superalloys differ — chemical composition, mechanical properties at room and elevated temperatures, corrosion performance across real industrial environments, heat treatment requirements, cost trade-offs, and application-specific selection guidance. Whether you are sourcing for an offshore oil platform, an aerospace OEM, or a chemical processing plant, you will leave with a clear procurement decision.

💡 The One-Sentence Rule

Inconel 625 = solid-solution strengthened, corrosion is the superpower.

Inconel 718 = precipitation-hardened, strength is the superpower.

This single metallurgical difference drives every decision below.

The 30-Second Decision Rule

Match your application to the right grade in one step:

🌊 Inconel 625

The Corrosion Champion

  • Seawater & marine

  • Chemical processing

  • Flue gas desulfurization

  • NACE MR0175 sour service

  • Weld overlay / cladding

  • No post-weld heat treatment

✈️ Inconel 718

The Strength Champion

  • Jet engine components

  • Gas turbine discs & blades

  • Cryogenic valve stems

  • High-strength fasteners

  • Nuclear reactor internals

  • 3D printed aerospace parts

Chemical Composition: The 9% Molybdenum Divide

The single biggest chemical difference between these two alloys is molybdenum. Inconel 625 contains approximately 9% Mo, while Inconel 718 contains only about 3% Mo. This difference fundamentally defines each alloy’s corrosion resistance profile.

Meanwhile, Inconel 718 compensates with niobium (Nb) at 5% — the key element that enables gamma-double-prime (γ”) precipitation hardening and makes 718 the strongest nickel alloy available.

ElementInconel 625 (wt%)Inconel 718 (wt%)Winner
Nickel (Ni)58.0 min50.0–55.0625 (higher Ni = better corrosion)
Chromium (Cr)20.0–23.017.0–21.0625 (slightly higher Cr)
Molybdenum (Mo)8.0–10.02.8–3.3625 (3× difference)
Niobium (Nb)3.15–4.154.75–5.50718 (key for γ” hardening)
Iron (Fe)5.0 maxBalance (~18)625 (lower Fe = better)
Titanium (Ti)0.40 max0.65–1.15718 (Ti aids γ’ hardening)
Aluminum (Al)0.40 max0.20–0.80718 (Al aids γ’ hardening)
Cobalt (Co)1.0 max1.0 maxTie

🧪 What This Tells You

625 invests its alloying budget in corrosion (Ni + Cr + Mo). 718 invests its alloying budget in strength (Nb + Ti + Al → precipitation hardening). The chemistry dictates the application. If your environment is aggressive chemically, stop reading and buy 625. If your application is strength-critical at temperature, keep reading about 718.

Mechanical Properties: Room Temperature

At room temperature, the strength difference is dramatic. Inconel 718 in the fully heat-treated (aged) condition achieves tensile strengths 30–40% higher than Inconel 625.

PropertyInconel 625 (Annealed)Inconel 718 (Aged)
Tensile Strength (UTS)827–1034 MPa (120–150 ksi)1275–1375 MPa (185–199 ksi)
Yield Strength (0.2% offset)414–655 MPa (60–95 ksi)1034–1165 MPa (150–169 ksi)
Elongation30–60%12–21%
Hardness170–230 HB331–415 HB (36–44 HRC)
Density8.44 g/cm³8.19 g/cm³
Modulus of Elasticity207 GPa (30,000 ksi)205 GPa (29,700 ksi)

Elevated Temperature Performance

Here’s where 718 truly shines. Above 540°C, the precipitation-hardened microstructure of 718 retains strength far better than the solid-solution structure of 625.

TemperatureInconel 625 Yield StrengthInconel 718 Yield StrengthAdvantage
Room Temp (20°C)517 MPa1100 MPa718 (+113%)
540°C (1000°F)380 MPa965 MPa718 (+154%)
650°C (1200°F)275 MPa860 MPa718 (+213%)
760°C (1400°F)125 MPa420 MPa718 (+236%)
870°C (1600°F)60 MPa150 MPa718 (+150%)

⚠️ Important Temperature Limit

At 650°C, 718’s γ” phase begins to coarsen and transform to stable δ phase, causing strength to drop. For sustained service above 650°C, consider Waspaloy, Inconel 740H, or Nimonic alloys instead. Inconel 625 retains better oxidation resistance above 870°C, though with reduced strength.

Corrosion Resistance: Where the Mo Difference Matters

Molybdenum is the decisive element for pitting and crevice corrosion resistance in chloride-containing environments. The PREN = %Cr + 3.3 × %Mo + 16 × %N formula tells the story:

  • Inconel 625: PREN ≥ 48 (20% Cr + 3.3 × 9% Mo + 16 × 0.02% N ≈ 49.8)
  • Inconel 718: PREN ≥ 26 (17% Cr + 3.3 × 3% Mo + 16 × 0.02% N ≈ 27.2)
  • For reference: 316L stainless steel: PREN ≥ 24
Corrosive EnvironmentInconel 625Inconel 718Notes
Seawater (flowing)⭐⭐⭐⭐⭐ Immune⭐⭐⭐ Good, limited data625 proven in 40+ years offshore
Seawater (stagnant/crevice)⭐⭐⭐⭐⭐ Immune⭐⭐ Crevice risk718 may corrode in stagnant seawater
Chloride SCC⭐⭐⭐⭐⭐ Immune⭐⭐⭐ Resistant (aged condition)Both far better than austenitic SS
H₂SO₄ (sulfuric acid)⭐⭐⭐⭐ Good to 40% @ RT⭐⭐⭐ Good to 20% @ RT625’s higher Ni helps in reducing acids
HCl (hydrochloric acid)⭐⭐⭐ Moderate at low conc.⭐ PoorNeither ideal for HCl without inhibitor
HNO₃ (nitric acid)⭐⭐⭐⭐ Excellent⭐⭐⭐ GoodBoth good in oxidizing acids
NACE MR0175 sour service⭐⭐⭐⭐⭐ Fully qualified⭐⭐⭐ Qualified (max 40 HRC)Both NACE approved; 718 hardness limited
Flue gas desulfurization⭐⭐⭐⭐⭐ Industry standard⭐⭐ Not recommended625 is the FGD reference material

Heat Treatment: One Hardens, One Doesn't

This is the single most important processing difference between 625 and 718, and it affects cost, lead time, and machinability strategy.

Inconel 625: Simple & Forgiving

625 is solid-solution strengthened. It does not require precipitation hardening. The standard heat treatment is a simple solution anneal:

980–1100°C
Solution Anneal

Quench
Water / Air

✅ Done
Ready to use

625 retains its properties even after welding — no post-weld heat treatment (PWHT) required. This dramatically reduces fabrication costs for large welded structures.

Inconel 718: Precise & Powerful

718 is precipitation-hardened via gamma-double-prime (γ”) and gamma-prime (γ’) phases. Achieving full strength requires a two-stage aging treatment:

980–1010°C
Solution @ 1 hr

Quench
Rapid cool

720°C / 8 hr
Stage 1 Aging

620°C / 8 hr
Stage 2 Aging

Air Cool
✅ Full Strength

625 Advantage

  • No aging = simpler processing

  • No PWHT after welding

  • Machine in final (annealed) condition

  • Lower processing cost

  • Faster turnaround

718 Requirement

  • Aging required (18 hr total)

  • PWHT after welding (restore strength)

  • Machine before aging (softer)

  • Higher processing cost

  • Longer lead time

Applications: Matching Grade to Industry

🛢️ Offshore Oil & Gas

Subsea manifolds, riser cladding, christmas tree components, umbilical tubing, and wellhead equipment. 625's NACE MR0175 qualification and seawater immunity make it the offshore standard. 718 used only for high-strength fasteners and valve stems where strength demands override corrosion requirements.

625 — Best Choice

✈️ Aerospace — Jet Engines

Compressor discs, turbine blades, casings, combustor hardware, and exhaust components. 718 dominates rotating parts where creep strength at 540–650°C is critical. Over 50% of a modern jet engine's weight can be Inconel 718. 625 is used for non-rotating parts (ducts, thrust reversers, bellows) where thermal fatigue matters more.

718 — Best Choice

⚗️ Chemical Processing

Reactors, heat exchangers, piping systems, and scrubbers handling mixed acids at moderate temperatures. 625's broad-spectrum corrosion resistance (oxidizing + reducing acids, chlorides) outperforms 718. Exception: 718 is used for high-temperature chemical valve internals above 500°C.

625 — Best Choice

💧 Marine & Desalination

Seawater pumps, desalination brine heaters, propeller shafts, and underwater connectors. 625 is the marine gold standard. 718 may be used in marine fasteners and shafts if crevice corrosion risk is controlled.

625 — Best Choice

☢️ Nuclear Power

Reactor internals, control rod mechanisms, hold-down springs, and core structural components. 718's combination of high strength + radiation resistance makes it the preferred material for PWR and BWR internals. 625 is used for corrosion-resistant cladding and welded overlays.

718 — Best Choice

💨 Gas Turbines (Land-Based)

Combustion cans, transition pieces, and turbine blades in industrial power generation turbines. 718's creep-rupture properties at 600°C are essential. 625 used for exhaust ducting and non-rotating hot section parts.

718 — Best Choice

⚒️ Flue Gas Desulfurization

Scrubber vessels, dampers, stack liners, and ducting in coal-fired and waste-to-energy power plants. 625 is the industry-standard FGD material — the aggressive sulfuric/chloride condensate environment demands PREN ≥ 48. 718 is not recommended.

625 — Best Choice

🔧 High-Strength Fasteners

Aerospace bolts, studs, and nuts requiring 180+ ksi strength at 540°C. 718 dominates because its precipitation-hardened microstructure delivers the highest bolting strength of any nickel alloy. 625 fasteners used where corrosion (not strength) drives the selection.

718 — Best Choice

Cost Comparison: Processing Drives the Premium

Both alloys are expensive relative to stainless steels, but 718 carries a 10–20% premium over 625. This premium comes from three sources:

Cost FactorInconel 625Inconel 718
Raw MaterialHigher Ni (58%), 9% Mo — ~$45-65/kgLower Ni (52%), 3% Mo, 5% Nb — ~$40-55/kg
Heat Treatment CostLow (simple anneal only)High (2-stage aging, 18 hours)
Fabrication (Welding)Low (no PWHT needed)High (PWHT required after welding)
MachiningModerate (annealed, ~190 HB)High (aged, ~350 HB; must machine pre-aging)
Estimated Total (plate)$45–95/kg$52–120/kg

💰 Total Cost of Ownership

While 718 costs 10-20% more to purchase, the total cost of ownership may favor 718 in wear-critical applications where longer service life offsets the initial premium. Conversely, 625’s no-PWHT advantage can save 15-25% on total fabrication cost for large welded assemblies. Request a quote for both grades and compare total delivered cost, not just material price.

Weldability & Machinability: Practical Differences

Inconel 625

  • Weldability: Excellent. The most weldable nickel superalloy. No PWHT required. ERNiCrMo-3 filler.
  • Weld cracking risk: Very low. Resistant to hot cracking due to Nb + Mo ratio.
  • Dissimilar welding: Preferred filler for welding 718 to itself and to other alloys.
  • Machinability: Moderate. Work hardens. Use carbide tooling at 25-30 m/min. Always machined in annealed condition.
  • Typical annealed hardness: ~190 HB — machinable with standard carbide tools.

Inconel 718

  • Weldability: Good, but PWHT required to restore strength after welding.
  • Weld cracking risk: Moderate. Strain-age cracking possible in highly restrained welds.
  • Dissimilar welding: Welded with ERNiCrMo-3 (625 filler) for best crack resistance.
  • Machinability: Difficult. Must machine before aging (solution-annealed, ~250 HB). Aged 718 at 36-44 HRC requires CBN or ceramic tooling.
  • Typical aged hardness: ~36-44 HRC — very difficult to machine. Pre-aging machining is standard practice.

Product Forms Availability

Product FormInconel 625Inconel 718
Sheet / PlateAMS 5599 — 0.5–76 mmAMS 5596 — 0.5–76 mm
Round BarAMS 5666 — 6–500 mm diaAMS 5662 / 5663 — 6–500 mm dia
Seamless TubeAMS 5581 — 6–219 mm ODAMS 5589 — 6–219 mm OD
Seamless PipeASTM B444 — up to 8″ NPSASTM B637 — limited sizes
ForgingsAMS 5666 — rings, discs, blocksAMS 5662 — rings, discs, blocks
Wire / Filler MetalERNiCrMo-3 — widely stockedERNiFeCr-2 — specialty item
Fittings / FlangesASTM B366 — widely availableSpecial order — longer lead time

Explore Inconel Products at Huaxiao Metal

Ready to source? We stock both grades with full MTC traceability:

Decision Framework: Which One Do You Need?

Use this table to match your operating conditions to the right grade:

Seawater Exposure

Any seawater immersion, splash zone, or marine atmosphere. 625's PREN ≥ 48 guarantees pitting and crevice corrosion immunity that 718 cannot match.

625

Mixed Acid Environments

Sulfuric + hydrochloric + nitric combinations. 625's high Ni + high Mo provides broad-spectrum corrosion resistance across oxidizing and reducing conditions.

625

FGD / Scrubber Service

Condensing acid environments in power plant scrubbers. 625 is the industry-standard reference material. Do not substitute 718.

625

Weld Overlay / Cladding

Overlaying carbon steel or low-alloy steel vessels and pipes. 625 (ERNiCrMo-3) is the universal choice — excellent weldability, no PWHT, seamless metallurgical bond. 718 is too crack-sensitive for cladding.

625

Service Above 540°C Under Load

Any rotating or load-bearing component above 540°C. 718 retains 2-3× the strength of 625 at temperature due to precipitation hardening.

718

Aircraft Engine Components

Compressor discs, turbine blades, casings, and rotating hardware. 718 is the #1 nickel alloy in aerospace by tonnage.

718

High-Strength Fasteners (180+ ksi)

Bolts, studs, and threaded components needing 180-200 ksi UTS at 540°C. 718 is the highest-strength bolting alloy commercially available.

718

Cryogenic Service (−196°C to −269°C)

718 retains exceptional toughness and strength at cryogenic temperatures (LNG, liquid hydrogen). Used for valve stems and structural components in cryogenic systems.

718

FAQ About Inconel 625 vs 718 Alloy

Inconel 625 is better for marine environments. Its 9% molybdenum content provides outstanding resistance to seawater corrosion, pitting (PREN ≥ 48), and chloride stress corrosion cracking. Inconel 718, while strong, does not have the same level of marine corrosion resistance and is primarily designed for high-temperature strength applications. For critical subsea and offshore equipment, 625 is the industry standard.

Inconel 718 is significantly stronger. When precipitation-hardened (aged), 718 achieves a tensile strength of up to 1375 MPa (199,000 psi) and yield strength of 1100 MPa (160,000 psi). Inconel 625 in annealed condition has a tensile strength of 827–1034 MPa (120,000–150,000 psi). 718 is approximately 30–40% stronger than 625 across its entire temperature range up to 650°C.

Yes, Inconel 625 and 718 can be welded together. The recommended filler metal is ERNiCrMo-3 (Inconel 625 filler) because it provides better weldability and cracking resistance. For 718 sections, post-weld heat treatment (aging) is required to restore strength. Inconel 625 is highly weldable and does not require PWHT, making 625 filler the preferred choice for dissimilar joints.

Inconel 718 is typically 10–20% more expensive than Inconel 625. Approximate pricing: Inconel 625 ranges from $45–95/kg depending on product form, while Inconel 718 ranges from $52–120/kg. The premium for 718 comes from more stringent heat treatment requirements (18 hours of two-stage aging), higher processing costs, and higher demand in aerospace applications. Both are significantly more expensive than standard stainless steels.

It depends on the specific component. Inconel 718 is the workhorse for rotating aerospace parts — compressor discs, turbine blades, fasteners, and casings where exceptional high-temperature strength (up to 650°C) is critical. Inconel 625 is preferred for aerospace ducting, exhaust systems, thrust reversers, and bellows where corrosion resistance and thermal fatigue resistance matter more than peak strength.

For Inconel 625: AMS 5599 (sheet/plate/strip), AMS 5666 (bar/forging), AMS 5581 (seamless tube).

For Inconel 718: AMS 5662 (bar/forging, solution treated + aged), AMS 5663 (bar/forging, direct aged), AMS 5596 (sheet/strip/plate), AMS 5589 (seamless tube).

These AMS specifications define the chemical, mechanical, and processing requirements for aerospace-grade material.

Inconel 625 is slightly easier to machine than Inconel 718 in the annealed condition. However, once 718 is precipitation-hardened (aged), it becomes significantly more difficult to machine — approaching 45 HRC hardness. Both alloys require carbide tooling, low cutting speeds (20–30 m/min), rigid setups, and generous coolant. Pre-hardening machining is standard practice for 718 components to minimize tool wear.

Huaxiao Metal supplies both Inconel 625 and Inconel 718 with full Mill Test Certificates (MTC) per EN 10204 3.1 or 3.2. We stock sheets, plates, bars, tubes, pipes, forgings, and fittings in both grades. All material is traceable to the original mill heat number. Contact us at [email protected] or WhatsApp +86-13761906384 for a quote within 12 hours.

Huaxiao Special Alloy Steel Products

Inconel 625 Alloy Tube Stock

Inconel 625

Inconel 625 (UNS N06625 / 2.4856) — The Corrosion Champion of Nickel Superalloys Best Seller — Best Corrosion Resistance Huaxiao Metal supplies Inconel 625 sheet,

Read More »
Finished 13-8 Mo stainless steel bright bars centerless ground AMS 5629

13-8 Mo Stainless Steel

13-8 Mo Stainless Steel Bar, Plate & Forging Supplier AMS 5629 / UNS S13800 / 1.4534 High-Strength PH Stainless Steel Huaxiao Metal supplies high-performance 13-8

Read More »
Incoloy Alloy 925 Bar

Incoloy Alloy 925

Incoloy Alloy 925 (UNS N09925) – Sheets, Plates, Bars, Pipes, Coils, Strips, Wires High-Strength Corrosion-Resistant Nickel Alloy Supplier & Manufacturer Incoloy 925 is a precipitation

Read More »
Incoloy Alloy 825 Sheet, Incoloy Metal Sheet

Incoloy 825

Incoloy 825 Alloy (UNS N08825) – Sheets, Plates, Bars, Pipes, Coils, Strips, Wires Corrosion Resistant Nickel-Iron-Chromium Alloy Supplier & Manufacturer Incoloy 825 alloy (UNS N08825)

Read More »
Incoloy 800 Suppliers, Incoloy 800 Prices

Incoloy 800

Incoloy 800 Alloy – Sheets, Plates, Bars, Pipes, Coils, Strips, Wires Incoloy 800 is part of our Incoloy alloy product range, which includes various nickel-iron-chromium

Read More »
Molybdenum Pipe

Molybdenum Metal & Alloys

Molybdenum Metal & Alloys Products – High-Quality Suppliers & Manufacturers | Huaxiao Metal Molybdenum-based materials—whether in the form of pure molybdenum metal, molybdenum alloys, or

Read More »
Tungsten Alloy Tubes, Tungsten Tubing

Tungsten Alloy

Tungsten Alloy Supplier – Rods, Plates, Sheets, Tubes, Wires & Custom Parts Tungsten alloy, also known as tungsten heavy alloy (WHA), is a high-density engineering

Read More »
Molybdenum Tube & Pipe Suppliers

Molybdenum Tube

Molybdenum Tube / Tubing & Pipe Supplier & Manufacturer – Huaxiao Metal Molybdenum tube, also known as molybdenum tubing or molybdenum pipe, is a high-performance

Read More »
Nimonic Alloy Strip

Nimonic Alloy

Nimonic Alloy 75, 80A, 90, 105 & 263 Supplier & Manufacturer At Huaxiao Metal, we are a trusted global supplier and manufacturer of Nimonic Alloys,

Read More »
cobalt alloy strip

Cobalt Alloy

Cobalt Alloys for High-Performance Applications | Global Supplier & Manufacturer Cobalt alloys are high-performance materials with exceptional strength, oxidation resistance, and corrosion resistance, even in

Read More »
Incoloy Alloy Bar Suppliers

Incoloy Alloy

Incoloy Alloy Supplier and Manufacturer From China Incoloy alloys are a class of corrosion-resistant and high-temperature alloys widely used in petrochemical, chemical processing, seawater treatment,

Read More »
monel alloy pipe, monel pipe suppliers

Monel Alloy

Monel Alloy Supplier and Manufacturer From China Huaxiao Metal is a professional Monel alloy supplier and manufacturer in China, specializing in Monel 400, Monel K-500,

Read More »
Inconel 718 Bar, 718 Inconel Alloy Bar

Inconel Alloy

Inconel Alloys — High-Performance Nickel-Based Superalloy Supplier | Huaxiao Metal We specialize in providing high-quality Inconel alloys to meet the needs of various industrial applications.

Read More »
Titanium Alloy Bar Suppliers

Titanium Alloy

Titanium Alloy Supplier: Grade 1-5 & Ti-6Al-4V Bars, Sheets, Plates | Huaxiao Metal Huaxiao Metal is a premier titanium alloy manufacturer and supplier with ISO9001

Read More »
Precision Alloy Bar

Precision Alloy

Precision Alloy Supplier | Invar, Kovar, Permalloy & Resistance Alloy Manufacturer Huaxiao Metal is a professional precision alloy manufacturer in China, providing high-performance functional alloys

Read More »
Precision slitting process of Hastelloy alloy coil at Huaxiao Metal factory

Hastelloy Alloy

Hastelloy Alloy – High Performance Nickel-Based Corrosion Resistant Alloy Supplier Reliable Hastelloy Alloy Manufacturer & Stockist | 15+ Years Global Export Experience When stainless steel

Read More »
High temperature alloys

High Temperature Alloy

High Temperature Alloy (Nickel-Based Superalloy) Supplier | Inconel, Hastelloy, GH Series – Available in Sheets, Bars, Pipes Huaxiao Metal is a premium high-temperature alloy manufacturer

Read More »

Share:

Facebook
Twitter
Pinterest
LinkedIn

Contact Us For Metal Prices

Table of Contents

On Key

Related Posts

Welcome